Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Horizontal |
PTS POM-90 Acetal Copolymer Information provided by PTS LLC. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ASTM D955 |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ASTM D955 |
PolyOne Dynaflex™ G7430-9001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**) Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 4.00 mm |
0.018 in/in @Thickness 0.157 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.20 mm |
0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.021 cm/cm @Thickness 3.20 mm |
0.018 - 0.021 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® SV1120M PBT Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.023 cm/cm | 0.018 - 0.023 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL004S is a compound based on Nylon 66 resin containing PTFE. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Time 86400 sec |
0.018 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Europe-Africa-Middle East) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® POM CO Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and Medium ViscosityInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GB10 L 10% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 HS N MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant, Nucleating Agent and Heat StabilizerFeatures: Lubricated, Fast Molding Cycle, Nucleated and Heat StabilizedTPCI# 8384101Information prov.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 NAT Availability: North AmericaForms: PelletsAppearance: Natural ColorTPCI# 8384101Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® POM CO TX10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%) and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® PA6/6 Nylon 66 Availability: North AmericaForms: PelletsFeatures: Low ViscosityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP PB006EQ PA 6 (Europe-Africa-Middle East) LNP *THERMOCOMP* PB006EQ is a compound based on PA 6 containing Glass Bead. Added features include Reduced Moisture. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 4.00 mm |
0.018 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin 100TL is a high viscosity acetal homopolymer containing 1.5% Teflo.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Clariant Renol POMSP0001 Acetal Copolymer, Aramid Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 4.00 mm |
0.018 - 0.022 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA6 D83 PA6, Injection Molded Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |