Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ASTM D955 |
Multibase Nylex™ 2112 FR V0 Natural Polyamide + PP Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE RCZ350D UV4 Thermoplastic Elastomer, UV-Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP HBK15030 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC GK8020 Polypropylene Copolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC GK8020 Polypropylene Copolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC T20020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC T3020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC T4020 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC TS16020 LE Polypropylene Copolymer, Mineral Reinforced, Low Emission Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS2020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 - 0.013 cm/cm | 0.0080 - 0.013 in/in | Injection; ISO 2257 |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | ASTM D955 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC T2020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC T8020 FC Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 HH-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Kolon KOPA® KN3311N General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | |
Polyram PlusTek PA352M6 Nylon 6.6, 30% Low Friction Mineral Filled 30% low friction mineral filled polyamide 6.6 lubricated with molybdenum for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | Flow direction; ASTM D955 |
Lubrizol Estane® 2355-55DE Thermoplastic Polyurethane Type: Pellethane® 2355-55DE is a thermoplastic polyurethane elastomer.Information Provided by The Lubrizol Corporation |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS3020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS8020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | as molded; ISO 294 |
LyondellBasell INDURE™ X210 TPO Description: INDURE™ X210 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, and processability. Appli.. |