Polymer Property : Linear Mold Shrinkage = 0.0110 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00518 cm/cm Grade Count:34
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Linear Mold Shrinkage 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00463 cm/cm Grade Count:23
Overview of materials for ABS/Polyester Alloy + GF
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage 0.00800 - 0.0110 cm/cm

@Temperature 121 - 121 °C
0.00800 - 0.0110 in/in

@Temperature 250 - 250 °F
Average value: 0.00950 cm/cm Grade Count:1
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage 0.00800 - 0.0110 cm/cm

@Time 1800 - 1800 sec
0.00800 - 0.0110 in/in

@Time 0.500 - 0.500 hour
Average value: 0.00950 cm/cm Grade Count:1
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage 0.00400 - 0.0110 cm/cm
0.00400 - 0.0110 in/in
Average value: 0.00760 cm/cm Grade Count:10
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.00450 - 0.0110 cm/cm
0.00450 - 0.0110 in/in
Average value: 0.00776 cm/cm Grade Count:43
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Linear Mold Shrinkage 0.00600 - 0.0110 cm/cm
0.00600 - 0.0110 in/in
Average value: 0.00900 cm/cm Grade Count:5
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.00100 - 0.0110 cm/cm
0.00100 - 0.0110 in/in
Average value: 0.00430 cm/cm Grade Count:51
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.00100 - 0.0110 cm/cm
0.00100 - 0.0110 in/in
Average value: 0.00326 cm/cm Grade Count:35
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Linear Mold Shrinkage 0.00100 - 0.0110 cm/cm
0.00100 - 0.0110 in/in
Average value: 0.00334 cm/cm Grade Count:62
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Linear Mold Shrinkage 0.00100 - 0.0110 cm/cm
0.00100 - 0.0110 in/in
Average value: 0.00341 cm/cm Grade Count:33
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..