Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm @Thickness 3.17 mm |
0.0015 - 0.0025 in/in @Thickness 0.125 in |
|
Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Dry Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0025 cm/cm | 0.0010 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0025 cm/cm | 0.0010 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0025 cm/cm @Thickness 3.17 mm |
0.0020 - 0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ PS-30GF/ 02S PBT Polyester - 30% Glass Fiber - 2% Silicone
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0025 cm/cm @Thickness 3.17 mm |
0.0020 - 0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® MLS-195A Polysulfone Alloy - ESD Material
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | ASTM D955 |
Sumitomo Bakelite North America SI 9041A Silicone Compound SI 9041A is a long fiberglass reinforced silicone molding compound, which exhibits excellent high temperature properties in addition to good molding characteristics for transfer and compression mold.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0025 cm/cm | 0.0020 - 0.0025 in/in | ASTM D955 |
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |