Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Network Polymers MS 160 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Network Polymers MS 175 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | |
Custom Resins Vexel™ E20GF45 FR , 45% Glass Reinforced, Flame Retardant PET
(discontinued **) Description: Vexel™ E20GF45 FR is a 45% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0070 cm/cm | 0.0020 - 0.0070 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 BR80 Nylon 6.6 for injection molding, 80% bronze filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | |
Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | |
Lord Adhesives Circalokâ„¢ 6715 Silicone Encapsulant Circalokâ„¢ 6715 is a two component, medium viscosity, solvent-free silicone which cures at room temperature to an elastomeric, stress-free rubber of outstanding electrical and high temperature p.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Eastman Eastar BR001 Copolyester Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D 955 |
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 4.00 mm |
0.0020 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 4.00 mm |
0.0020 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 GV 35 HWCP 35% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | |
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | ASTM D-955 |
Axiall NR-5009 Rigid PVC, Molding Georgia Gulf NR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent processability, .. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0336G20CL Glass Reinforced Coupled |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0336G25M5CL Glass/Mineral Reinforced Coupled |
|||
Linear Mold Shrinkage | 0.0020 - 0.014 cm/cm | 0.0020 - 0.014 in/in | ASTM D955 |
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® NI-40GF/000 Nylon 6/10 - 40% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Asahi Kasei Delpet® 60N Acrylic Molding Compound 60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
Samsung Cheil Industries Starex® HF-5661H ASA, Unreinforced
(discontinued **) Amorphous Styrene Acrylonitrile (SAN)Characteristics: High Flow: Impact, Heat and Chemical Resistance and Surface GlossApplications: Pens, TV Components, Refrigerator and Appliance ComponentsProcess.. |