Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
0.012 - 0.025 in/in
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing..
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
0.012 - 0.025 in/in
SABIC PP 5702P Polypropylene Homopolymer for Injection Molding
Product Description: PP 5702P is specially developed for rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical..
Linear Mold Shrinkage 0.020 - 0.025 cm/cm
0.020 - 0.025 in/in
ISO 294-4
Premix Thermoplastics PRE-ELEC® 12-000
PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a..
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
0.012 - 0.025 in/in
FRISETTA Test Method
Nilit FRIANYL B63 V2 Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, flame retardant.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
0.012 - 0.025 in/in
SABIC PP 57MNK10 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 57MNK10 is a controlled rheology PP grade of medium molecular weight distribution specially developed for producing injection molded articles. This grade has an excellent i..
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
PolyOne Lubri-Tech™ AT-000/5T Black Acetal-Copolymer, PTFE Lubricated  (discontinued **)
Preliminary DataDescription/Features:PTFE LubricatedInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade  (discontinued **)
Suggested fabrication methods: Fiber spinningFeatures: High speed spinning, Improved bulk, Low gas fadeTypical applications: Upholstery, BCF carpet yarnsComplies with FDA specification, Title 21, CF..
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Ineos H00M-00 Polypropylene Homopolymer  (discontinued **)
Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, Enhanced flow, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical applications..
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Ineos H38G-01 Polypropylene Homopolymer, Fiber Grade  (discontinued **)
Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fadeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical pr..
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
BP Amoco Acctuf® 3143 Impact Copolymer Polypropylene  (discontinued **)
Suggested fabrication methods: Sheet extrusion; Thick-wall Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injectio..
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Linear Mold Shrinkage 0.018 - 0.025 cm/cm
0.018 - 0.025 in/in
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Ineos H20Z-03 Polypropylene Homopolymer
This is a homopolymer containing nucleation and antistatic. It is designed for injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520...
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Ineos H36G-00 Polypropylene Homopolymer
This is a high flow rate homopolymer. This material is designed for fiber spinning and spun bonded processes. It meets the requirements of the U.S. Food and Drug Administration as specified in 21 ..
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
Lehmann & Voss PLASLUBE NY-1/TF/20/BK Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Linear Mold Shrinkage 0.0080 - 0.025 cm/cm
0.0080 - 0.025 in/in
ASTM D955
Cheng Yu Plastic 3235 TPE Rubber
Linear Mold Shrinkage 0.0080 - 0.025 cm/cm
0.0080 - 0.025 in/in
ASTM D955
Cheng Yu Plastic 3276 TPE Rubber
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Ineos H20E-00 Polypropylene Homopolymer
This is a homopolymer containing antistatic designed for injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Application..
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
BP Amoco Acctuf® 3240 Impact Copolymer Polypropylene  (discontinued **)
Suggested fabrication methods: Extrusion; Fiber Optic CableFeatures: NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
BP Amoco Acclear® 8449 Random Copolymer Polypropylene, High Clarity Grade  (discontinued **)
Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlTypical applications: Housewares, Rigid packagingComplies wit..
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
BP Amoco Amoco® 6361 Polypropylene Homopolymer  (discontinued **)
Suggested fabrication methods: Extrusion; Blow moldingFeatures: Ease of processingTypical applications: Oriented film, Sheet, Fiber, Profile, Consumer productsComplies with FDA specification, Title ..
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Ineos H35G-01 Polypropylene Homopolymer  (discontinued **)
Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520...
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Ineos H38K-00 Polypropylene Homopolymer, Fiber Grade  (discontinued **)
Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fade, Low smokeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520..