Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
NatureWorks® Ingeo™ 3801X Injection Grade PLA Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP HBK15030 D Polypropylene, Multifiller High Gloss, Detergent Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PP HBK15030 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC T20020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS4020D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 W-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ NH11L Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | (longitudinal) Injection; ISO 2257 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | ASTM D955 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC K6020 S Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC T8020 FC Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH BK901213 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 - 0.013 cm/cm | 0.0080 - 0.013 in/in | |
Lehmann & Voss LUVOCOM® 1105-8320 PEEK, with aramid reinforcement and PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | ASTM D955 |
Kolon Kopa® KN161 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Kolon KOPA® KN333HS Heat Resistant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Kolon KOPEL® KP3755 Specialty TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.013 cm/cm | 0.0070 - 0.013 in/in | |
Lehmann & Voss LUVOCOM® 1/AR/5/NT Polyamide 66, with aramid reinforcement Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Isotropic shrinkage characteristics.Control disks, cams, s.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Kolon KOPA® KN3311N General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | GB/15585 |
Zhejiang Juner JEPP2007 PP For Automotive Parts Applications: Inner Decorate PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Linear Mold Shrinkage | 0.0040 - 0.013 cm/cm | 0.0040 - 0.013 in/in | ASTM D955 |
Beijing Ranger Chem PBT-201-G15 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | ASTM D955 |
Beijing Ranger Chem PBT-201-G10 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | as molded; ISO 294 |
LyondellBasell INDURE™ X210 TPO Description: INDURE™ X210 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, and processability. Appli.. |