Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.0110 cm/cm | 0.00200 - 0.0110 in/in | Average value: 0.00518 cm/cm Grade Count:34 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0110 cm/cm | 0.00200 - 0.0110 in/in | Average value: 0.00463 cm/cm Grade Count:23 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0110 cm/cm @Temperature 121 - 121 °C |
0.00800 - 0.0110 in/in @Temperature 250 - 250 °F |
Average value: 0.00950 cm/cm Grade Count:1 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0110 cm/cm @Time 1800 - 1800 sec |
0.00800 - 0.0110 in/in @Time 0.500 - 0.500 hour |
Average value: 0.00950 cm/cm Grade Count:1 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0110 cm/cm | 0.00400 - 0.0110 in/in | Average value: 0.00760 cm/cm Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.00450 - 0.0110 cm/cm | 0.00450 - 0.0110 in/in | Average value: 0.00776 cm/cm Grade Count:43 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.0110 cm/cm | 0.00600 - 0.0110 in/in | Average value: 0.00900 cm/cm Grade Count:5 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0110 cm/cm | 0.00100 - 0.0110 in/in | Average value: 0.00430 cm/cm Grade Count:51 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0110 cm/cm | 0.00100 - 0.0110 in/in | Average value: 0.00326 cm/cm Grade Count:35 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0110 cm/cm | 0.00100 - 0.0110 in/in | Average value: 0.00334 cm/cm Grade Count:62 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0110 cm/cm | 0.00100 - 0.0110 in/in | Average value: 0.00341 cm/cm Grade Count:33 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |