Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00503 cm/cm Grade Count:58 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Linear Mold Shrinkage | 0.000800 - 0.00800 cm/cm | 0.000800 - 0.00800 in/in | Average value: 0.00547 cm/cm Grade Count:7 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00552 cm/cm Grade Count:106 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00450 cm/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00800 cm/cm | 0.00500 - 0.00800 in/in | Average value: 0.00628 cm/cm Grade Count:15 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | -0.00100 - 0.00800 cm/cm | -0.00100 - 0.00800 in/in | Average value: 0.00220 cm/cm Grade Count:107 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00455 cm/cm Grade Count:174 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00800 cm/cm | 0.000500 - 0.00800 in/in | Average value: 0.00304 cm/cm Grade Count:14 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00319 cm/cm Grade Count:7 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.00800 cm/cm | 0.000200 - 0.00800 in/in | Average value: 0.00255 cm/cm Grade Count:21 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00800 cm/cm | 0.00500 - 0.00800 in/in | Average value: 0.00675 cm/cm Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00313 cm/cm Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00467 cm/cm Grade Count:19 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00335 cm/cm Grade Count:27 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.00150 - 0.00800 cm/cm | 0.00150 - 0.00800 in/in | Average value: 0.00526 cm/cm Grade Count:248 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00468 cm/cm Grade Count:11 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00504 cm/cm Grade Count:104 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00500 cm/cm Grade Count:8 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00250 - 0.00800 cm/cm | 0.00250 - 0.00800 in/in | Average value: 0.00517 cm/cm Grade Count:75 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00150 - 0.00800 cm/cm | 0.00150 - 0.00800 in/in | Average value: 0.00356 cm/cm Grade Count:13 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00543 cm/cm Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |