Polymer Property : Linear Mold Shrinkage = 0.0045 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
LATI
LATI LAPEX A G/10 10% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)  (Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
PolyOne Therma-Tech™ NJC-6500 Nylon 12  (discontinued **)
PolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned
Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
RHODIA-EP
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® 160D S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® 185A L series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® 185A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® 198A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® S190A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® S195A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® S385A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
RHODIA-EP
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0
Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® 190A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber
Heat stabilized, 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
Adell BR-14 Nylon 6, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
Adell BR-34 Nylon 6, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
restricted
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned)
Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
Adell AR-14 Nylon 66, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
restricted
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
ISO 2577
Polyram PlusTek RA325G4 Nylon 66 for Injection Molding, 20% Glass-Fiber Reinforced, Self-Extinguishing, Halogen Free
20% Glass-fiber reinforced, self-extinguishing halogen free Nylon 66 for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® 385A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
Polyram PlusTek PB312J6 Nylon 6, 30% Glass Fiber
30% glass-fiber reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
SK Chemicals SKYTHANE® 195A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..