Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018EB is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films. Availability: Africa & Middl.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP) AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
Dow DOWLEX™ 2025G Linear Low Density Polyethylene DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
Dow ELITE™ 5401G Enhanced Polyethylene Resin ™ 5401G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking for excellent performance on a.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. .. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | target |
Bapolene® 108A Low Density Polyethylene Film Extrusion Resin Bapolene® 108A is an LDPE for blown film. It contains 2500 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin (European Grade) Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high clarity film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impa.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil Exceed™ 2018EB Blown Film Resin
(discontinued **) Exceed 2018EB resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals Exxpol® Technology. The higher melt index makes this polymer ideally sui.. |
|||
Antiblock Level | 2500 ppm | 2500 ppm | |
ExxonMobil Exceed™ 1018 EB Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |