Polymer Property : Particle Size = 40 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size <= 40 µm
<= 40 µm
90% smaller than
Nyco NYGLOS® 8 Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
Particle Size 40 µm
40 µm
mesh.
Oceanchem Group Sodium Formate 95-96% powder
Molecular Formula: NaCOOHInformation Provided by Oceanchem Group
Particle Size 40 µm
40 µm
Average Diameter
Potters Industries Conduct-O-Fil® SA300S20 Silver-coated Aluminum Granules
Applications:EMI shielding in contact with aluminumConductive adhesivesAerospace and marine applicationsAdvantages:Low density with high conductivityLow galvanic corrosion in contact with aluminumIn..
Particle Size 40 - 60 µm
40 - 60 µm
Lucite International Colacryl ® D150 Acrylic Dental Resin
A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f..
Particle Size 40 µm
40 µm
Shin-Etsu Silicones KMP-400 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Particle Size 40 µm
40 µm
Silberline Sparkle Silver® 3624
Sparkle Silver® 3624 is a coarse, brilliant, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a w..
Particle Size >= 40 µm
>= 40 µm
250 Mesh; PS-1-2
Solvay JAGUAR® HP 8FF Surfactant
Description: Hydroxypropyl guar with extremely low residue, designed to be easily dispersed into water where it will wet out and hydrate, forming a viscous HPG fluid which will readily crosslink wit..
Particle Size <= 40 µm
<= 40 µm
Thru #100 Mesh; RP-0499
Solvay REPEL-O-TEX® PF-594 Surfactant
Description: High active soil release polymer for powder laundry. Prevents adhesion of soils between washes and soil redeposition during wash. Repel-O-Tex PF 594 has been specifically formulated for..
Particle Size 40 µm
40 µm
at a density of 2.10 g/cc, pressure 2.5 t/cc
TIMCAL TIMREX® GB99/6 Natural Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Particle Size 40 - 55 µm
40 - 55 µm
d90, Guaranteed
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Particle Size 40 - 50 µm
40 - 50 µm
d90, Guaranteed
TIMCAL TIMREX® C-LUB 310 Primary Synthetic Graphite
Information provided by TIMCAL
Particle Size <= 40 µm
<= 40 µm
Max
CIMBAR Miti-Wite B10 Chemically Purified White Barite (BaSO4)
Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes ..
Particle Size 40 µm
40 µm
D90
Dandong Taico Minerals TAICOCITE® TC3 Magnesium Hydroxide
Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®..
Particle Size <= 40 µm
<= 40 µm
Max
CIMBAR BariScan Ultra Chemically Purified White Barium Sulfate (BaSO4)
BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requireme..
Particle Size <= 40 µm
<= 40 µm
Max
CIMBAR CIMBAR™ 325 Barite Powder (BaSO4)
CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical ..
Particle Size 40 µm
40 µm
Average
Azoty Tarnow™ TARFLEN SM-B40 PTFE
Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Particle Size 40 µm
40 µm
Average
Azoty Tarnow™ TARFLEN SM-G15 PTFE
Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Particle Size 40 µm
40 µm
Average
Azoty Tarnow™ TARFLEN SM-G20 PTFE
Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Particle Size 40 µm
40 µm
Average
Azoty Tarnow™ TARFLEN SM-S15 PTFE
15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Particle Size 40 µm
40 µm
Average
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE
Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Particle Size 40 µm
40 µm
Average
Azoty Tarnow™ TARFLEN SM-S25 PTFE
Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Particle Size 40 µm
40 µm
Effective Top Size
3M iM16K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 40 µm
40 µm
50th%
3M K46 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 40 µm
40 µm
50th%
3M S35 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 40 µm
40 µm
50th%
3M S38 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 40 µm
40 µm
D50
3M S38XHS Glass Bubbles
3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik..
Particle Size 40 µm
40 µm
95" Percentile
3M W-610 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..
Particle Size 40 µm
40 µm
50th%
3M D32/4500 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 40 µm
40 µm
Average Diameter
Potters Industries Conduct-O-Fil® SA300S30 Silver-coated Aluminum Granules
Applications:EMI shielding in contact with aluminumConductive adhesivesAerospace and marine applicationsAdvantages:Low density with high conductivityLow galvanic corrosion in contact with aluminumIn..
Particle Size 40 µm
40 µm
Average Diameter
Potters Industries Conduct-O-Fil® SM40P20 Silver-coated Magnetic Particles
Applications:EMI shieldingConductive adhesivesZ-axis conductive filmsAdvantages:Alternative to nickel when neededParticles can be magnetically alignedHalf the density of silver-coated nickelInformat..