Polymer Property : Bulk Density = 0.0134 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.370 g/cc
0.0134 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons CORAX® N 330 ASTM Carbon Black
Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons.
Bulk Density 0.370 g/cc
0.0134 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons ECORAX® 1990 Carbon Black
Specialty black for tire treads and bodies that provide reduced rolling resistanceInformation provided by Orion Engineered Carbons.
Bulk Density 0.370 g/cc
0.0134 lb/in³
Zircar Zirconia YF-100 Yttria Felt Insulation
Yttria (yttrium oxide - Y2O3) is typically used as a stabilizer for zirconia. It is offered here in its pure and stable metal oxide form, which is not attacked by most molten metals, including lithi..
Bulk Density 0.370 - 0.430 g/cc
0.0134 - 0.0155 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable
Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning ..
Bulk Density >= 0.370 g/cc
>= 0.0134 lb/in³
LSY-QB-KD019
LG Chemical PA828 Processing aid
Description: High molecular weightApplication: Foam, soft product etcInformation provided by LG Chemical
Bulk Density >= 0.370 g/cc
>= 0.0134 lb/in³
LSY-QB-KD019
LG Chemical PA930 Processing aid
Description: Ultra high molecular weightApplication: Foam, soft product etcInformation provided by LG Chemical
Bulk Density 0.370 g/cc
0.0134 lb/in³
Zircar Zirconia YF-100 Yttria Felt Insulation
Yttria (yttrium oxide - Y2O3) is typically used as a stabilizer for zirconia. It is offered here in its pure and stable metal oxide form, which is not attacked by most molten metals, including lithi..
Bulk Density 0.370 g/cc
0.0134 lb/in³
Daikin POLYFLON L-2 PTFE Low Polymer, White Fine Powder
White fine powder.Major Uses: Suited especially to applications requiring fine dispersion of particles. Mold lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, p..
Bulk Density 0.370 - 0.450 g/cc
0.0134 - 0.0163 lb/in³
Akzo Nobel Expancel® 930 MB 120 Masterbatch with unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Bulk Density 0.370 g/cc
0.0134 lb/in³
Asahi Glass Fluon® L169J PTFE Lubricant
Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As..
Bulk Density 0.370 g/cc
0.0134 lb/in³
ASTM D1895
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer
This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire..
Bulk Density 0.370 g/cc
0.0134 lb/in³
ASTM D1895
ALM TPE-210-S Prototyping Polymer
A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and ab..
Bulk Density 0.370 g/cc
0.0134 lb/in³
ASTM D4894-98a
3M Dyneon™ TF 1750 PTFE
Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very ..