LG Chemical PA828 Processing aid

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical PA828 Processing aid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: High molecular weightApplication: Foam, soft product etcInformation provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Bulk Density >= 0.370 g/cc
>= 0.0134 lb/in³
LSY-QB-KD019
Volatiles <= 1.0 %
<= 1.0 %
ISO 1625
Particle Mesh Size 35 Mesh
35 Mesh
<2% (mesh on); LSY-QB-KD018
200 Mesh
200 Mesh
<2% (mesh pass); LSY-QB-KD018
Viscosity Measurement 4.3 - 5.2
4.3 - 5.2
ISO 3105
Thermal Properties Metric English Comments
Melting Point >= 132 °C
>= 270 °F
Flash Point 490 °C
914 °F
Descriptive Properties Value Comments
Foreign Material <3% (10 x 10 cm)
LSY-QB-KD005
Fusion time 55-70 sec
ISO 8130-6