Material Notes:
Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 0.370 - 0.430 g/cc
0.0134 - 0.0155 lb/in³
After drying at 110°C
Particle Size <= 7000 µm
<= 7000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 0.300 - 0.500 MPa

@Temperature 815 °C
43.5 - 72.5 psi

@Temperature 1500 °F
Cold Crushing Strength
0.400 - 0.600 MPa

@Temperature 100 °C
58.0 - 87.0 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.0300 - 0.0900 W/m-K

@Temperature 100 °C
0.208 - 0.625 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.100 - 0.160 W/m-K

@Temperature 600 °C
0.694 - 1.11 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.120 - 0.180 W/m-K

@Temperature 815 °C
0.833 - 1.25 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Maximum Service Temperature, Air 870 °C
1600 °F
Shrinkage -3.00 - 1.00 %

@Temperature 815 °C
-3.00 - 1.00 %

@Temperature 1500 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 9.0 %
9.0 %
SiO2 33 %
33 %
Descriptive Properties Value Comments
ASTM Classification N
Material Consumption per 1 m3 320 kg
Mixing Water 120-170 liters
per 100 kgs dry material