Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | Tapped |
Nyco 10 AS WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | Tapped |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
Nabaltec NABALOX® NO 201P Soft Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-109JS PET Sheet Grade Used mainly for 5 to 20 liter mineral water containers |
|||
Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-113C PET Sheet Grade Used mainly for box strapping. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | DIN 53466 |
3M Dyneon™ PFA 6502TA Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6502TA is a fluorothermoplastic resin developed for compression molding applications. PFA 6502TA has a wide processing window with excellent color stability when longer residence times or.. |
|||
Bulk Density | <= 0.850 g/cc | <= 0.0307 lb/in³ | |
Magyar Aluminum ALOLT 38AF Aluminum Hydroxide Ground type |
|||
Bulk Density | <= 0.850 g/cc | <= 0.0307 lb/in³ | |
Magyar Aluminum ALOLT 720 Aluminum Hydroxide Viscosity Optimized Type |
|||
Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
Sharadaa Ceramics 60LBD Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL 7 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Bulk Density | <= 0.850 g/cc | <= 0.0307 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL ZAP-014 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | DIN 53466 |
Stanelco Bioplast® Wrap 100 Biodegradable Plastic Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 32245 Phenolic, Injection Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | ASTM D1895 |
Plenco 6343 Phenolic, Granular, Compression Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
Daikin NEOFLON AC-5830 PFA Coating Powder, Gray NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.Info.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF Ultraform® E 3120 BM POM Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF Ultraform® N2650 Z4 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | DIN 53466 |
3M Dyneon™ PFA 6502 TAZ Perfluoroalkoxy Fluorothermoplastic Granules 3M™ Dyneon™ PFA 6502TAZ is a fluorothermoplastic resin for compression molding applications. PFA 6502TAZ has a wide processing window with excellent color stability when longer residence times or .. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | Tapped |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF Ultraform® N2520 XL2 POM Description: Is a POM, injection-molding grade with increased electrical conductivity, for applications with reduced mechanical requirements.Information provided by BASF |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | Powder Density; ASTM D1895 |
Sumitomo Bakelite North America TEM 9053C Hardware Grade Epoxy Short fiberglass and mineral filled, toughened epoxy molding compound with excellent dimensional stability and high strength properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | ASTM D4894-98a |
3M Dyneon™ TF 1620 PTFE Meets ASTM D4894 Type IV, Grade 2 resinSemi-free-flowing compression molding powderHigh bulk densityGood for large billets and thin walled isostatic moldingsVery dense polymer structure, similar to .. |