Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® LN 3000 Expandable Polystyrene Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® EH 2000 Expandable Polystyrene Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is use.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® EH 3000 Expandable Polystyrene Extir EH 3000 is an expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 3000 is u.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene
(discontinued **) Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene
(discontinued **) Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **) Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene
(discontinued **) Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene
(discontinued **) Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene
(discontinued **) Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® E 5000 AE Expandable Polystyrene
(discontinued **) Extir E 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or H.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® F 1111 Expandable Polystyrene
(discontinued **) Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® P 1212 Expandable Polystyrene
(discontinued **) Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. .. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
SGL Carbon Group CF 270 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Silon TA 2347 HD Orange Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2347 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System... |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Silon Taborex TA 2329 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1117 HD. TA 2329 HD contains a cross-linking catalyst and a stabiliser package. Together with the above-mentioned grafted P.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Zircar Ceramics IB-100A Alumina Bubble Thin wall aluminum oxide ceramic spheres offered in 2 standard bubble sizes. These low density sintered ceramic bodies are useful in a range of refractory applications with temperatures to 2000°C (.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | Tap |
TIMCAL TIMREX® T150-600 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ISO 60 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | Loose |
Nyco ULTRAFIBRE® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® EH 5000 Expandable Polystyrene Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® LN 2000 Expandable Polystyrene Extir LN 2000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Plenco 7321 Phenolic, Nodular, Compression Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |