Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Extir®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of blowing agent. Extir CM does not contain CFC or HCFC. Extir CM Galileo Europa 5 AE contains an atherman additive that reduces heat transfer, and the items produced with it, gray in color, have excellent thermal insulation properties. Its unique formula allows the use of thinner boards to achieve the same thermal resistance.Applications: Extir CM Galileo Europa 5 AE reaches the top performances as thermal insulation. It is highly recommended for all applications in which thickness is a limiting factor: cavity wall insulationfloor insulating boards.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Bulk Density 0.590 - 0.630 g/cc
0.0213 - 0.0228 lb/in³
Density >= 0.0120 g/cc
>= 0.000434 lb/in³
Minimum apparent density on a continuous pre-expander after two expansions
>= 0.0160 g/cc
>= 0.000578 lb/in³
Minimum apparent density on a discontinuous pre-expander
>= 0.0180 g/cc
>= 0.000650 lb/in³
Minimum apparent density on a continuous pre-expander after one expansion
0.0120 - 0.0250 g/cc
0.000434 - 0.000903 lb/in³
Density range normally used
Particle Size 900 - 1600 µm
900 - 1600 µm