Material Notes:
Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir F 1111 exhibits an excellent surface finishing. This feature, combined with a low gas emissions and residual carbon during the casting operation, will guarantee optimal quality of the final metallic parts.Applications: Extir F 1111 is a special grade developed for lost foam casting technology. It exhibits an excellent processability and surface finishing. Typical casting applications are aluminium engine blocks, engine manifolds, and other cast engine parts.It is recommended to keep the product in a dry well ventilated store between 15-20°C. For product packaged in octabins the guaranteed shelf-life is one month; product in steel drums has a six months guaranteed shelf-life. During the processing of Expandable Polystyrene any sparkle or flame must be avoided and smoking should be forbidden. An adequate electrical grounding of machinery and of pneumatic transport lines is recommended. For further information concerning storage, packaging and processing precautions please refer to "Styrenics - Technical data sheets" and to the "Extir Safety Data Sheet". This grade complies by composition with the requirements set by the main regulations for plastics intended for food contact (including the EEC directive 90/128).Processing: Extir F 1111 can be easily pre-expanded over a wide density range from 20 to 35 kg/m³. The recommended ageing time before moulding obviously depends on the pre-expanded density and ranges from 6 to 24 hours. Extir F 1111 is also an easy mould filling product. The low energy needs of Extir F 1111 means that it can be moulded with fast cycles (mainly by decreasing the water and vacuum cooling times).Information provided by Polimeri Europa
Physical Properties Metric English Comments
Bulk Density 0.590 - 0.630 g/cc
0.0213 - 0.0228 lb/in³
Density 0.0210 - 0.0350 g/cc
0.000759 - 0.00126 lb/in³
Apparent Bulk Density 0.0200 g/cc
0.000723 lb/in³
On a discontinuous pre-expander
0.0240 g/cc
0.000867 lb/in³
On a continuous pre-expander after one expansion
Particle Size 200 - 500 µm
200 - 500 µm