Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0077 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0077 cm/cm

@Time 86400 sec
0.0077 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK
LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am..
Linear Mold Shrinkage, Transverse 0.0077 cm/cm

@Time 86400 sec
0.0077 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA
LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
Linear Mold Shrinkage, Transverse 0.0077 cm/cm

@Time 86400 sec
0.0077 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific)
LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0077 cm/cm

@Time 86400 sec
0.0077 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RVL28 PA 66
LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura..