Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear .. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC (Asia Pacific) LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC LNP* STAT-KON* DE0029 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DX01303C PC LNP STAT-KON* DX01303C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0039 cm/cm @Time 86400 sec |
0.0039 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific) LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |