Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.76 - 1.95 g/cc | 0.0636 - 0.0704 lb/in³ | |
Pyrotek Dense Fused Silica Pre-Cast Shapes Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, coppe.. |
|||
Density | 1.90 - 1.95 g/cc | 0.0686 - 0.0704 lb/in³ | |
Pyrotek Pyrocast AR PLUS Castable Refractory Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed... |
|||
Density | 1.80 - 1.95 g/cc | 0.0650 - 0.0704 lb/in³ | |
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.85 - 1.95 g/cc | 0.0668 - 0.0704 lb/in³ | |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.75 - 1.95 g/cc | 0.0632 - 0.0704 lb/in³ | Molded |
Bulk Molding Compounds BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Density | 1.75 - 1.95 g/cc | 0.0632 - 0.0704 lb/in³ | Molded |
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap.. |
|||
Density | 1.90 - 1.95 g/cc | 0.0686 - 0.0704 lb/in³ | |
Pyrotek Pyrocast XL Small Component Refractory ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast.. |
|||
Density | 1.03 - 1.95 g/cc | 0.0372 - 0.0704 lb/in³ | Average value: 1.72 g/cc Grade Count:31 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |