Physical Properties Metric English Comments
Density 1.10 - 1.10 g/cc

@Temperature 325 - 325 °C
0.0397 - 0.0397 lb/in³

@Temperature 617 - 617 °F
Average value: 1.10 g/cc Grade Count:1
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Density 0.00310 - 1.10 g/cc
0.000112 - 0.0397 lb/in³
Average value: 0.108 g/cc Grade Count:273
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Density 0.980 - 1.10 g/cc
0.0354 - 0.0397 lb/in³
Average value: 1.04 g/cc Grade Count:84
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Density 0.700 - 1.10 g/cc
0.0253 - 0.0397 lb/in³
ASTM B212
H.C. Starck Amperit® 847.6 Agglomerated Yttria (Y2O3)
Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
5% Lucobit in Bitumen B50/70
Lucobit Lucobit® 1210A Ethylene Copolymer Bitumen
Lucobit 1210A is a mixture of ethylene copolymers and special bitumen. Addition of Lucobit to bitumen increases its viscosity and broadens the range of plasticity.Lucobit 1210A in asphalt mixtures ..
Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
2.4% Lucolast in Bitumen B50/70
Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive
Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticit..
Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
Solvay GEROPON® TK 32 Surfactant
Description: GEROPON TK-32 is an effective dispersant in liquid formulationsChemical Name: SODIUM N-METHYL-N-TALL OIL TAURATECAS: 61791-41-1, 67-63-0Solubility in water: SolubleAvailable in: Asia Pa..
Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
Solvay MIRACARE® SLB-205/N Surfactant
Description: Miracare SLB-205/N is a free flowing, high active surfactant concentrate used in the preparation of structured liquids. It is a surfactant base used to stabilize additives applied in a ..
Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
RP-17617
Solvay MIRACARE® SLB-365/G Surfactant
Description: Miracare® SLB-365/G is a complete formulated system containing mild anionic and amphoteric foaming surfactants and a structuring agent in an easy to use lamellar concentrate. Upon di..
Density 1.06 - 1.10 g/cc
0.0383 - 0.0397 lb/in³
AV15
Solvay Amyl Acid Phosphate
Identification: AMYL ACID PHOSPHATE - Phosphoric acid, mono – and bis –(branched and linear pentyl esters)CAS: 84418 – 71 – 3Available in: Asia Pacific, Europe, Latin America and..
Density 0.0280 - 1.10 g/cc
0.00101 - 0.0397 lb/in³
Average value: 0.876 g/cc Grade Count:36
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Density 1.06 - 1.10 g/cc
0.0383 - 0.0397 lb/in³
Average value: 1.07 g/cc Grade Count:9
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma..
Density 1.10 - 1.10 g/cc

@Temperature 325 - 325 °C
0.0397 - 0.0397 lb/in³

@Temperature 617 - 617 °F
Average value: 1.10 g/cc Grade Count:1
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Density 0.947 - 1.10 g/cc
0.0342 - 0.0397 lb/in³
Average value: 1.00 g/cc Grade Count:18
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
Copyright © lookpolymers.com All Rights Reserved