| Category | Ceramic , Oxide |
| Manufacturer | H.C. Starck |
| Trade Name | Amperit® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | H.C. Starck Amperit® 847.6 Agglomerated Yttria (Y2O3).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.700 - 1.10 g/cc | 0.0253 - 0.0397 lb/in³ | ASTM B212 |
| Particle Size | 38 µm | 38 µm | Maximum of 5% less than |
| 45 µm | 45 µm | Maximum of 10% less than | |
| 106 µm | 106 µm | Maximum of 10% greater than | |
| 125 µm | 125 µm | Maximum of 2% greater than |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Aluminum, Al | <= 0.020 % | <= 0.020 % | |
| Calcium, Ca | <= 0.020 % | <= 0.020 % | |
| Carbon, C | 1.0 - 1.5 % | 1.0 - 1.5 % | |
| Iron, Fe | <= 0.050 % | <= 0.050 % | |
| Molybdenum, Mo | <= 0.010 % | <= 0.010 % | |
| Silicon, Si | <= 0.10 % | <= 0.10 % | |
| Y2O3 | 98.2 - 99 % | 98.2 - 99 % | |
| Zirconium, Zr | <= 0.10 % | <= 0.10 % |