Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.921 - 0.970 g/cc | 0.0333 - 0.0350 lb/in³ | Average value: 0.931 g/cc Grade Count:191 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Density | 0.945 - 0.970 g/cc | 0.0341 - 0.0350 lb/in³ | ASTM D792 |
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®. |
|||
Density | 0.964 - 0.969 g/cc | 0.0348 - 0.0350 lb/in³ | ASTM D4052 |
ExxonMobil Jayflex™ DIDP (0.2% BPA) Plasticizer (European Grade) Availability: Europe, Middle East & AfricaInformation provided by ExxonMobil |
|||
Density | 0.965 - 0.970 g/cc | 0.0349 - 0.0350 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ DIDP Plasticizer Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-49-1Information provided by ExxonMobil |
|||
Density | 0.964 - 0.968 g/cc | 0.0348 - 0.0350 lb/in³ | ASTM D4052 |
ExxonMobil Jayflex™ DIDP Plasticizer (European Grade) Availability: Europe, Middle East & AfricaCAS Number: 68515-49-1EC Number: 271-091-4Information provided by ExxonMobil |
|||
Density | 0.965 - 0.970 g/cc | 0.0349 - 0.0350 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ DIDP-E Plasticizer Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-49-1Information provided by ExxonMobil |
|||
Density | 0.960 - 0.970 g/cc @Temperature 20.0 °C |
0.0347 - 0.0350 lb/in³ @Temperature 68.0 °F |
|
Oceanchem Group Tri-isobutyl Phosphate (TIBP) Molecular Formula: C12H27O4PCas No.: 126-71-6Chemical Properties: Ester property, it can be hydrolyzed in basic condition.Hazardous Features: It can be fired in heat, fire and oxidation condition, a.. |
|||
Density | 0.939 - 0.970 g/cc | 0.0339 - 0.0350 lb/in³ | Average value: 0.951 g/cc Grade Count:130 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Density | 0.940 - 0.970 g/cc | 0.0340 - 0.0350 lb/in³ | Average value: 0.957 g/cc Grade Count:48 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |