Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.907 - 0.910 g/cc @Temperature 20.0 °C |
0.0328 - 0.0329 lb/in³ @Temperature 68.0 °F |
1st Grade |
Kazanorgsintez Alpha-Methylstyrene Fraction Production Method: Alpha-methylstyrene fraction is a by-product of the production of phenol and acetone by the cumene method. Application: Used for the production of marketable alpha-methylstyreneIn.. |
|||
Density | 0.860 - 0.910 g/cc | 0.0311 - 0.0329 lb/in³ | RP-0549 |
Solvay RHODOLINE® DF-665 Surfactant Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis BA11CF Polypropylene Copolymer BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. .. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis BB213CF Polypropylene Copolymer BB213CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BB213CF is recommended for food packaging.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis BD712CF Polypropylene Copolymer BD712CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD712CF is recommended for food packaging.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Borclear™ RB707CF Polypropylene Random Copolymer for Blown Film Borclear RB707CF is a propylene-ethylene copolymer film resin without slip and antiblock additives, suitable for the manufacturing of unoriented film on blown film process.Borclear RB707CF is especi.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Borclear™ RB709CF Polypropylene Ethylene Copolymer Borclear™ RB709CF is a propylene -ethylene copolymer. This grade is suitable for the manufacturing of unoriented film on blown film lines. Applications: Borclear™ RB709CF is recommended for seal.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Borclear™ RD738CF Propylene Alpha Olefin Copolymer for Cast Film Borclear RD738CF is a slip and antiblock formulation propylene alpha olefin copolymer resin. It is suitable for the manufacturing of unoriented film on chill roll process.Borclear RD738CF is suitabl.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Borclear™ RE718CF Propylene Alpha Olefin Copolymer for Metallizable Cast Film Borclear RE718CF is a propylene alpha olefin copolymer resin formulation with antiblocking agent and without Ca-stearate, especially developed for the manufacturing of unoriented cast films for meta.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Bormed™ TD109CF Polypropylene Copolymer Bormed™ TD109CF is a propylene alpha olefin copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: lamination films, food.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Bormod™ HD905CF Polypropylene Homopolymer for Cast Film Bormod HD905CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, suitable for the manufacturing of unoriented film on chill roll process. It is recomme.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film Bormod HD915CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, especially developed for the manufacturing of unoriented film for metallizing. It is s.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
Borealis BorPure™ RD226CF Polypropylene Random Copolymer BorPure™ RD226CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD226CF is recommended for food packaging.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer BorPure™ RD266CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD266CF is recommended for
food packaging.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis BorPURE™ RE216CF Polypropylene Random Copolymer BorPure™ RE216CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: BorPure™ RE216CF is recommended for Lamination films, Me.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Borseal™ RE239CF Polypropylene Copolymer Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Daploy™ WB180HMS Polypropylene Daploy™ WB180HMS is a propylene-based, structurally isomeric polymer.Information provided by Borealis AG |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
Borealis HD204CF Polypropylene HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
Borealis HD234CF Polypropylene HD234CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD234CF is recommended for food packaging, lamination films, stationery f.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
Borealis HD244CF Polypropylene HD244CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationery folders, multi layer co-extr.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
Borealis HD601CF Polypropylene HD601CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: metallisable cast film, inner layer in co extrusion, textile packaging fil.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
Borealis HD621CF Polypropylene HD621CF is a polypropylene homopolymer This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
Borealis HD822CF Polypropylene HD822CF is a polypropylene homopolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
Borealis RD204CF Polypropylene Random Copolymer RD204CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD204CF is recommended for blending, food packaging, high qua.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis RD461CF Polypropylene Random Copolymer RD461CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD461CF is recommended for food packaging, high quality stati.. |
|||
Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi.. |
|||
Density | 0.862 - 0.910 g/cc | 0.0311 - 0.0329 lb/in³ | Average value: 0.885 g/cc Grade Count:16 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |
|||
Density | 0.880 - 0.910 g/cc | 0.0318 - 0.0329 lb/in³ | RP-17617 |
Solvay RHODOLINE® 679 Surfactant Description: Highly effective mineral oil defoamer for latex processing.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 679 is recommended for application at 0... |