| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.908 g/cc | 0.0328 lb/in³ | ASTM D792 |
|
Multibase Multi-Flex® TPE A 8502-SR BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
|
|||
| Density | 0.907 g/cc | 0.0328 lb/in³ | ASTM D792 |
|
Network Polymers NPP 30-1200
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
|
|||
| Density | 0.907 g/cc | 0.0328 lb/in³ | ASTM D792 |
|
Network Polymers NPP 30-1200 A
Description: Homopolymer Polypropylene Nucleated with AntistaticInformation provided by Network Polymers Inc.
|
|||
| Density | 0.907 g/cc | 0.0328 lb/in³ | ASTM D792 |
|
Network Polymers NPP 30-2000 NA
Description: Homopolymer Polypropylene Nucleated with AntistatInformation provided by Network Polymers Inc.
|
|||
| Density | 0.909 g/cc | 0.0328 lb/in³ | ASTM D4883 |
|
Eastman 812A Polyethylene
(discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not..
|
|||
| Density | 0.909 g/cc | 0.0328 lb/in³ | ASTM D4883 |
|
Eastman 812P Polyethylene
(discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet...
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | ASTM D1505 |
|
LyondellBasell Montell 8340 Polybutene-1
Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | ASTM D1505 |
|
LyondellBasell Montell 8640 Polybutene-1
Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements..
|
|||
| Density |
0.907
-
0.910
g/cc @Temperature 20.0 °C |
0.0328
-
0.0329
lb/in³ @Temperature 68.0 °F |
1st Grade |
|
Kazanorgsintez Alpha-Methylstyrene Fraction
Production Method: Alpha-methylstyrene fraction is a by-product of the production of phenol and acetone by the cumene method. Application: Used for the production of marketable alpha-methylstyreneIn..
|
|||
| Density | 0.907 g/cc | 0.0328 lb/in³ | ISO 1183 |
|
IPB Bicell® Cellular Polypropylene Sheet
Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe..
|
|||
| Density | 0.909 g/cc | 0.0328 lb/in³ | ASTM D1505 |
|
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s..
|
|||
| Density | 0.909 g/cc | 0.0328 lb/in³ | ASTM D1505 |
|
Lushan M-20A Adhesive Resin for Multi-layer Oxygen Barrier Pipe
Adhesive resin Lushan series for multi-layer oxygen barrier pipe is a modified polyolefin with functional groups. It’s designed to bond to a variety of barrier materials, such as nylon and ethy..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | |
|
Silon Tabond 3012 Adhesive Resin
TABOND 3012 is an LLDPE based adhesive resin.Characteristics: • Highest adhesion to aluminium, copper, brass and steel • Adhesion durability at elevated temperatures and pressure cycling p..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | ISO 1183 |
|
Borealis BC545MO Polypropylene Copolymer
BC545MO is a low-blush polypropylene heterophasic copolymer intended for injection molding. This grade features high impact strength, high thermal stability and very good process ability. As all pol..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | ISO 1183 |
|
Borealis HD120MO Polypropylene
HD120MO is a polypropylene homopolymer with a good combination of mechanical properties intended for injection molding. Applications: sanitary equipment, caps and closures, and general packagingInf..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | ISO 1183 |
|
Borealis HE125MO Polypropylene
HE125MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by good flow properties and high stiffness in and is specially suitable for high-speed injection mo..
|
|||
| Density | 0.909 g/cc | 0.0328 lb/in³ | ASTM D1505 |
|
Westlake EC812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bin..
|
|||
| Density | 0.909 g/cc | 0.0328 lb/in³ | ASTM D1505 |
|
Westlake EM812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi..
|
|||
| Density |
0.908
g/cc @Temperature 15.6 °C |
0.0328
lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
|
ExxonMobil Synesstic™ 5 Synthetic Fluid
Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stabilit..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | |
|
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
AFFINITY® PL 1840 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown film products with low temperature sealability, excellent puncture resistance, outstanding blown f..
|
|||
| Density | 0.909 g/cc | 0.0328 lb/in³ | ASTM D792 |
|
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to provide blown film with low temperature sealability, good puncture resistance, optics and..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | ASTM D297 |
|
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber
Description: This crystalline ethylene-propylene-diene terpolymer (EPDM) has a low viscosity for excellent flow characteristics and hot green strength. It has been designed for property modification..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | |
|
ConocoPhillips 680 Gear Oil AGMA Lubricant No. 8EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Density |
0.908
g/cc @Temperature 23.0 °C |
0.0328
lb/in³ @Temperature 73.4 °F |
ISO 1183 |
|
Arkema Group OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene
OREVAC C306 is anhydride modified LLDPE. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. It has been designed..
|
|||
| Density | 0.907 g/cc | 0.0328 lb/in³ | ASTM D1505 |
|
Amco PRIMATOP PP HOMO 120NA-HF Multi-Purpose Polypropylene
Features:medium viscosityexcellent processabilitygood stiffnessnucleationanti-statApplications:closuresthin wall applicationshousewaresFormer A-Top Polymers product; part of Amco product line since ..
|
|||
| Density | 0.907 g/cc | 0.0328 lb/in³ | |
|
ConocoPhillips 32 Soluble Oil
Description: Conoco Soluble Oil is a general-purpose oil suited for a wide variety of cutting and grinding operations that require a combination water-soluble lubricant and coolant. Soluble Oil is a..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | ISO 1183 |
|
Borealis HF136MO Polypropylene
HF136MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by a good combination of mechanical and flow properties. This polymer is a CR (controlled rheology..
|
|||
| Density | 0.909 g/cc | 0.0328 lb/in³ | ASTM D792 |
|
Ineos H07G-00 Polypropylene Homopolymer
Grade H07G-00 is a barefoot polypropylene homopolymer designed for cast film applications and flexible packaging. This grade has good optical properties and consistent processing. This grade meets t..
|
|||
| Density | 0.908 g/cc | 0.0328 lb/in³ | ASTM D792 |
|
Dow Engage® 8540 Polyolefin Elastomer
Description: Engage® 8540 polyolefin elastomer is an ethyleneoctene copolymer that is well suited to foamed applications and offers excellent performance for profile extrusion of tubing and hoses. ..
|
|||
| Density | 0.907 g/cc | 0.0328 lb/in³ | ISO 1183 |
|
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
Bormed HD810MO is a specially modified polypropylene homopolymer intended for use in medical and medical related applications, which have to be sterilized by radiation. Products molded in HD810MO a..
|
|||