| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density |
0.907
-
0.910
g/cc @Temperature 20.0 °C |
0.0328
-
0.0329
lb/in³ @Temperature 68.0 °F |
1st Grade |
|
Kazanorgsintez Alpha-Methylstyrene Fraction
Production Method: Alpha-methylstyrene fraction is a by-product of the production of phenol and acetone by the cumene method. Application: Used for the production of marketable alpha-methylstyreneIn..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis BA11CF Polypropylene Copolymer
BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. ..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis BD212CF Polypropylene Copolymer
BD212CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD212CF is designed for food packaging, l..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Borclear™ RB707CF Polypropylene Random Copolymer for Blown Film
Borclear RB707CF is a propylene-ethylene copolymer film resin without slip and antiblock additives, suitable for the manufacturing of unoriented film on blown film process.Borclear RB707CF is especi..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Borclear™ RB709CF Polypropylene Ethylene Copolymer
Borclear™ RB709CF is a propylene -ethylene copolymer. This grade is suitable for the manufacturing of unoriented film on blown film lines. Applications: Borclear™ RB709CF is recommended for seal..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Borclear™ RE718CF Propylene Alpha Olefin Copolymer for Metallizable Cast Film
Borclear RE718CF is a propylene alpha olefin copolymer resin formulation with antiblocking agent and without Ca-stearate, especially developed for the manufacturing of unoriented cast films for meta..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Bormed™ TD109CF Polypropylene Copolymer
Bormed™ TD109CF is a propylene alpha olefin copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: lamination films, food..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Bormod™ HD905CF Polypropylene Homopolymer for Cast Film
Bormod HD905CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, suitable for the manufacturing of unoriented film on chill roll process. It is recomme..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film
Bormod HD915CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, especially developed for the manufacturing of unoriented film for metallizing. It is s..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
|
Borealis BorPure™ RD226CF Polypropylene Random Copolymer
BorPure™ RD226CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD226CF is recommended for food packaging..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
|
Borealis BorPure™ RD234CF Polypropylene Random Copolymer
BorPure™ RD234CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD234CF is recommended for food packaging, stationa..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer
BorPure™ RD266CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD266CF is recommended for
food packaging..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis BorPURE™ RE216CF Polypropylene Random Copolymer
BorPure™ RE216CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: BorPure™ RE216CF is recommended for Lamination films, Me..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Borseal™ RE239CF Polypropylene Copolymer
Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Daploy™ WB180HMS Polypropylene
Daploy™ WB180HMS is a propylene-based, structurally isomeric polymer.Information provided by Borealis AG
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
|
Borealis HD204CF Polypropylene
HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
|
Borealis HD234CF Polypropylene
HD234CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD234CF is recommended for food packaging, lamination films, stationery f..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
|
Borealis HD601CF Polypropylene
HD601CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: metallisable cast film, inner layer in co extrusion, textile packaging fil..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
|
Borealis HD621CF Polypropylene
HD621CF is a polypropylene homopolymer This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
|
Borealis HD822CF Polypropylene
HD822CF is a polypropylene homopolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis RD461CF Polypropylene Random Copolymer
RD461CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD461CF is recommended for food packaging, high quality stati..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis RD734CF Polypropylene Random Copolymer
RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stati..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis BorPURE™ RD208CF Polypropylene Random Copolymer
BorPure™ RD208CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. This grade is suitable for the manufacturing of unoriented films o..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film
Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | base resin; ISO 1183 |
|
Borealis RD735CF Polypropylene Random Copolymer
RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging ..
|
|||
| Density | 0.862 - 0.910 g/cc | 0.0311 - 0.0329 lb/in³ | Average value: 0.885 g/cc Grade Count:16 |
|
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a..
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis HD214CF Polypropylene Homopolymer
HD214CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationary films, multi layer co-extrus..
|
|||
| Density | 0.880 - 0.910 g/cc | 0.0318 - 0.0329 lb/in³ | RP-17617 |
|
Solvay RHODOLINE® 679 Surfactant