Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.76 g/cc | 0.316 lb/in³ | Theoretical |
Kennametal Stellite Stellite® STAR cast Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy Characteristics:Because of the wide melting range, this filler metal has good gap filling characteristics at the lower end of the brazing range and is relatively free-flowing near the upper end. We.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Lucas-Milhaupt Silvaloy® 30 Brazing Alloy Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stai.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged 1300 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged at 538°C (1000°F) for 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | Annealed |
Eagle Brass 752 Nickel Silver 18%, 1/4 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | Annealed |
Eagle Brass 752 Nickel Silver 18%, Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
CLAL-MSX NICLAL 1800 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
CLAL-MSX NICLAL 1800 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
CMW® 353 Copper Alloy CMW® 353 material is an economical high strength, high conductivity copper base alloy. It is a heat treatable copper base alloy and its excellent properties are obtained largely through heat treatm.. |
|||
Density | 8.74 g/cc | 0.316 lb/in³ | |
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Density | 8.74 g/cc | 0.316 lb/in³ | |
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Density | 8.74 g/cc | 0.316 lb/in³ | |
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Density | 8.74 g/cc | 0.316 lb/in³ | |
Carpenter HyMu "80"® Electronic Alloy, Strip, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Density | 8.75 g/cc | 0.316 lb/in³ | |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |