Physical Properties Metric English Comments
Density 8.48 g/cc
0.306 lb/in³
Lucas-Milhaupt BRAZE 051 Silver Based Cadmium Free Filler Metal
Characteristics:Braze 051 is a low cost, intermediate temperature silver brazing filler metal suitable for joining various ferrous and non-ferrous alloys that can be heated to 1650EF/900EC without d..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, aged 1000 hours at 982°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, all-weld metal, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, mill annealed
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.47 g/cc
0.306 lb/in³
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Density 8.48 g/cc
0.306 lb/in³
Theoretical
Kennametal Stellite Deloro® N-6 PM with P/M Processing
Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing ..
Density 8.47 g/cc
0.306 lb/in³
Indium Corp. Indalloy 27 Bismuth Solder Alloy
Information Provided by Indium Corporation
Density 8.47 g/cc
0.306 lb/in³
Special Metals INCONEL® Alloy 600
A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for..
Density 8.46 g/cc
0.306 lb/in³
Wall Colmonoy COLMONOY® 228 Custom Formulated Nickel-Based Alloy For Glass
Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Application: FusewelderInformation pro..
Density 8.47 g/cc
0.306 lb/in³
Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy
Finished product available as wire, rod, or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extrude..
Density 8.47 g/cc
0.306 lb/in³
Chicago Extruded Metals UNS C33500 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in bars.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Density 8.47 g/cc
0.306 lb/in³
Chicago Extruded Metals UNS C34500 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in rods.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Density 8.47 g/cc
0.306 lb/in³
Chicago Extruded Metals UNS C35300 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals
Density 8.47 g/cc
0.306 lb/in³
Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Density 8.48 g/cc
0.306 lb/in³
Theoretical
Kennametal Stellite Deloro® N-6 PM cast
Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing ..