Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.40 - 8.60 g/cc | 0.303 - 0.311 lb/in³ | |
PSM Industries Pacific Sintered Metals Copper CU-143-W Powdered Metal High electrical and thermal conductivity, Good for heat sinks and electrical problemsInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | P/M (98%) |
Kennametal Stellite Deloro® 208 PM after P/M Processing Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | P/M (97%); 8.64 g/cc theoretical |
Kennametal Stellite Stellite® 3 PM with P/M Processing Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt.. |
|||
Density | 8.38 g/cc | 0.303 lb/in³ | theoretical |
Kennametal Stellite Stellite® 6 PM with P/M Processing Adhesive wear test data: 0.49 P/M, 0.48 Cast; Typical applications include: (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) die.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy Denertia™ C4 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.It conforms to the following International Standards: EN 1641 §4... |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Wall Colmonoy COLMONOY® 4 - Hard-Surfacing Alloy With Chromium Boride Description: Contains wear-resistant chromium borides and carbides. Has greater impact resistance and workability than Colmonoy No.5. Finished with carbide tools and grinding.Method of Application.. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Weartech International WT-6 Cobalt Hardfacing & Wear Resistant Alloy Applications: engine valves, pump shafts & sleeves, hot cutting & rotary knives, high pressure high temperature valves, extrusion screwsInformation provided by Weartech International |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Goodfellow Iron 50/Nickel 50 Alloy Information provided by Goodfellow. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Goodfellow Iron 55/Nickel 45 Alloy Low Nickel magnetic alloy. Most applications are based on the requirements of moderately high saturation and permeabilities greater than silicon irons. Uses include the manufacture of sensitive rela.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy Information provided by Goodfellow. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Goodfellow Nickel 52/Iron 48 Alloy Used in magnetic and glass-metal seal applicationInformation provided by Goodfellow. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Universal Wire Works No. 6 Cobalt Alloy Welding Wire Universal No. 6 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme impact resistance at elevated temperatures, exhaust valve contact surfaces, hot and cold trimmer dies an.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C (1350°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C/8hr/FC to 621°C/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Alliance S-20B Samarium Cobalt Magnetic Material |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Alliance S-28A Samarium Cobalt Magnetic Material |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Alliance S-28B Samarium Cobalt Magnetic Material |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Alliance S-30A Samarium Cobalt Magnetic Material |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Alliance S-30B Samarium Cobalt Magnetic Material |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Plus Aging 649°C (1200°F)/4hr/FC to 579°C/4hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 718°C (1325°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
AIM 63Sn/Pb37 Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Alliance S-26H Samarium Cobalt Magnetic Material |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 746°C (1375°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Density | 8.40 g/cc | 0.303 lb/in³ | |
Alliance S-22B Samarium Cobalt Magnetic Material |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
HP Alloys HPA COBALT Alloy 6B, Wear Resistant, (Co-Cr-W) (UNS R30016) Cobalt 6B is a cobalt based chromium, tungsten alloy for wear environments where seizing, galling and abrasion are present. 6B is resistant to seizing and galling and with its low coefficient of fri.. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
HP Alloys HPA COBALT Alloy 6BH, Wear Resistant, (Co-Cr-W) (UNS R30016) Cobalt 6BH is the same composition of Cobalt 6B, except the material is hot rolled and then age hardened. The direct age-hardening after hot rolling provides the maximum hardness and wear resistance.. |