Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.78 - 3.85 g/cc | 0.137 - 0.139 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9816 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 BR80 Nylon 6.6 for injection molding, 80% bronze filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
Parker Chomerics CHO-FLEX 4432 Conductive Ink CHO-FLEX polyester inks were developed for the membrane keyboard and sensor industries. The ink bond to Mylar films, and can be creased, heat-formed or scratched without affecting their performance... |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
GBC Grade 98 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
Microplasmic Anodizing [Ceramic Coating] for Aluminum, Magnesium, Titanium, Zirconium & Composites Microplasmic Process is for all types of aluminum, magnesium, titanium and zirconium alloys and composite materials. It is an electrochemical micro arc oxidation process for which a U.S. pat.. |
|||
Density | 3.80 - 4.60 g/cc | 0.137 - 0.166 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 512.059 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12 |
|||
Density | 3.80 - 4.50 g/cc | 0.137 - 0.163 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 512.074 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12 |
|||
Density | 3.80 - 4.40 g/cc | 0.137 - 0.159 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 518.001 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Density | 3.80 - 4.40 g/cc | 0.137 - 0.159 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 518.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Density | 3.80 - 4.40 g/cc | 0.137 - 0.159 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 526.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Density | 3.80 - 4.40 g/cc | 0.137 - 0.159 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 526.077 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Density | 3.80 - 4.80 g/cc | 0.137 - 0.173 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 544.059 Dense Coated Tungsten Carbide-Nickel 83-17 (WC-Ni) |
|||
Density | 3.80 - 4.40 g/cc | 0.137 - 0.159 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60) Composition is of NiSF RC 60 only |
|||
Density | 3.80 - 4.40 g/cc | 0.137 - 0.159 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 560.077 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60) Composition is of NiSF RC 60 only |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
CeramTec Ziralit Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 CeramTec's Zirconia Toughened Alumina (Ziralit) provides excellent strength, excellent temperature performance, and superior toughness. It has enhanced performance for high quantity volume productio.. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | ASTM-C 20 |
CoorsTek CAP 4 98.5% Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | ASTM C20 |
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
Cotronics Duralco™ 120 500°F Silver Filled Epoxy, Electrically Conductive Contains over 70% ultra fine silver to provide excellent electrical conductivity. Cures at room temperature.>Applications: ideal for use where maximum conductivity is required. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Dry) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | Side 2, Silicone Property; Arlon SQA-TMS-024 |
Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical value.. |
|||
Density | >= 3.80 g/cc | >= 0.137 lb/in³ | |
Advanced Ceramics ACL 1085 (C-795) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
Density | 3.78 g/cc | 0.137 lb/in³ | ASTM-C20 |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
Density | 3.78 g/cc | 0.137 lb/in³ | DIN EN 993: part 2 |
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance) Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn.. |
|||
Density | 3.80 g/cc | 0.137 lb/in³ | |
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
Density | 3.80 - 3.88 g/cc | 0.137 - 0.140 lb/in³ | extruded; ASTM D792 |
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon PTFE G Standard Compound with bronzeProperties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |
|||
Density | 3.80 - 5.20 g/cc | 0.137 - 0.188 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 526.059 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Density | 3.80 - 4.60 g/cc | 0.137 - 0.166 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 529.074 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo) |