Physical Properties Metric English Comments
Density 3.80 - 4.80 g/cc
0.137 - 0.173 lb/in³
ASTM B417
Particle Size 8.0 - 13 µm
8.0 - 13 µm
10%
16 - 23 µm
16 - 23 µm
50%
30 - 37 µm
30 - 37 µm
90%
Component Elements Properties Metric English Comments
Carbon, C 5.0 - 5.2 %
5.0 - 5.2 %
Nickel, Ni 16 - 18 %
16 - 18 %