Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.80 g/cc | 0.101 lb/in³ | |
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Pyrotek Pyrocast ZEAL Refractory Shapes Aggregate Base: MulliteApplicationsDoor sill Furnace ramp Crucible bottom / lining Information provided by Pyrotek. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
PEAK Werkstoff DISPAL S691 Aluminum Alloy, AlCu5Ti High stiffness and elongation at ruptureInformation provided by PEAK Werkstoff GmbH |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Apparent |
Gouda Vuurvast AK 85 KM Dense Refractory Brick Description: This brick based on mullite and corundum, is characterized by a very low porosity, high slag resistance, low creep and very good thermal shock resistance.Remarks: This data represents a.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Schott GM27884 Dental Glass Remarks: Ba-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Schott GM39923 Dental Glass Remarks: Ba- and F-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide.. |
|||
Density | 2.80 g/cc @Temperature 20.0 °C |
0.101 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Flux Drystatic Potassium Fluoroaluminate Flux using electrostatic/dry powder coating. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & .. |
|||
Density | 2.80 - 3.00 g/cc @Temperature 20.0 °C |
0.101 - 0.108 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Flux P2 Potassium Fluoroaluminate Mixtures of NOCOLOK® Flux P2 with NOCOLOK® Flux allow for gradual viscosity adjustments in suspensions to suit specific process conditions.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automoti.. |
|||
Density | 2.80 g/cc @Temperature 20.0 °C |
0.101 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Flux Potassium Fluoroaluminate A high quality fluxing agent for brazing aluminum components. Classifications: HS No.: 38109090/CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration .. |
|||
Density | 2.80 - 3.00 g/cc @Temperature 20.0 °C |
0.101 - 0.108 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Li Flux Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Frequenta® Steatite Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Vista Metals Duramold-2™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Goodfellow Dural® Aluminum /Copper/Magnesium Alloy High strength, low weight alloy; in the solution heat-treated and aged condition, mechanical properties are as good as, or better than, low-carbon steel. Limited weldability. Used in aircraft and ae.. |
|||
Density | 2.79 g/cc | 0.101 lb/in³ | |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Du-Co Ceramics DC-200-L-5 Fosterite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
COI Ceramics Nextel™ AS-N650 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-B30 PTFE Reinforced with 30% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon CP-594CX Bulk Compound Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but .. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
ALIMEX ACP 6000 Aluminum Cast Plate Aluminum cast plate ACP 6000 is a 7xxx series alloy surface-machined plate. This type of alloy ensures excellent machinability characteristics and adequate tensile strength. Thickness, flatness and .. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Alpase M-1™ Aluminum Mold Plate M-1™ features and benefits include: Dimensional stability, fully weldable, anodizable, consistent hardness - regardless of size, can be nickel plated, good machinability, no heat treatment required.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
BASF Paliotol™ Yellow K 1700 Color Additive Type of Pigment: Azo pigment, Ca/Na Lake Recommendations for food applications: Germany and FranceApplications: LDPE, HDPE/PP, PVC-P, PVC-U, PS, ABSInformation provided by BASF |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib.. |