Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 33C (7.80 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 33C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |