Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP 5C003 FP-V (PVDF) LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp 5C003 LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Techmer ES HiFill® TPX-HTN-02028 A 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66 (Asia Pacific) LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
UCAR Carbon UCAR® CHV Extruded Graphite Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular proper.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Toho Tenax Besfight® G30-500 12K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.76 - 1.88 g/cc | 0.0636 - 0.0679 lb/in³ | ASTM D792 |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Plenco 6500 Phenolic, Briquette, Transfer Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Loctite® 3532 High viscosity Dam Encapsulant COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® 1SVX-65H black 9288 PA1010-GF65 Product Description: Grilamid 1SVX-65H black is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources Exc.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65 Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® TW241F12 (COND) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Cytec Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Chem Polymer Durlex 740-10 GB PBT, 40% Short Glass Fiber, 10% Glass Bead Reinforced A 40% short glass fiber, 10% glass bead reinforced PBT, offering a combination of tensile strength, warpage control and dimensional stability for close tolerance applications.Data provided by the ma.. |
|||
Density | 1.76 - 1.96 g/cc | 0.0636 - 0.0708 lb/in³ | Molded |
Bulk Molding Compounds BMC HT12-1027 Unsaturated Polyester Bulk Molding Compound BMC HT12-1027 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 31508/0009 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31508/0009 also has a very low brittleness temperatu.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 1960B-1 is a mineral and short fiberglass filled epoxy compound, formulated for the encapsulation of passive electronic devices.Information provided by Sumitomo Bak North America, Inc. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 31008/0003 Polyvinylidene Fluoride
(discontinued **) 3M™ Dyneon™ PVDF 31008/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31008/0003 also has a very low brittleness temperatu.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 32008/0000 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesInformation provided by Dyneon, A 3M.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Techmer ES HiFill® PVDF CF10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |