Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF30 FR NAT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill® ABS 1067 Availability: North AmericaFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM HO 0167 S1 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hGR40 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP IF00C PA6.12 LNP* THERMOCOMP* IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America 775 CAF Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183-87 |
Wellman Wellpet® FRGF116-BK1 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Polyram RamSter PE321G6 PET, 30% Glass Fiber, Flame Retardant 30% Glass fiber reinforced, flame retardant V-0 PET for injection molding applications.Information provided by Polyram. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D542-90 |
DuPont™ Kapton® 150FN019 Polyimide/FEP Composite Film 150 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Eurostar Starpylen HU 70E4 ECR Starpylen HU 70E4 ECR is a Renewable Calcium Carbonate (oyster shell) Masterbatch in a PP carrier. Engineered to reduce carbon footprint in mineral filled compound.Information provided by Eurostar. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET 30% Glass Fiber Reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
BASF Petra® 330 FR BK-112 30% Glass Filled PET Petra 330 FR BK-112 is a 30% glass reinforced, flame retardant PET, pigmented black injection molding compound rated UL94 V-0 in a 1/64 inch thickness. The product is designed for injection molding.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |