Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | DIN 53479; ASTM D792 |
Kolon SPESIN® KP212G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | Crystalline; ISO 1183 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copolymer LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Techmer ES Luriblend® POM CO GF10 TL10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Techmer ES Plaslube® J-50/30/TF/10 Polycarbonate, 30% GFR, 10% PTFE Plaslube glass fiber reinforced polytetrafluorethylene (PTFE) lubricated polycarbonate grades have an excellent balance of mechanical strength characteristics, dimensional stability and wear and fri.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK LNP THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP fo.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF009H PA 66 (Asia Pacific) LNP* Thermocomp* RF009H is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Polyram RamSter PF306G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | Nominal Laminate Density |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/48280/1000 Fabric Fiber: T1000 12K 5H Satin, 283 g/m2Information provided by HexCel |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 926-82-1 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Polyplastics Duranex® 3300H Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HTV-4H1 black 9205 PA6T/6I-GF40 Product description: Grivory HTV-4H1 black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 GB4 POM 20% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |