Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792, ISO 1183 |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPHC K2040H Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.23 - 1.47 g/cc | 0.0444 - 0.0531 lb/in³ | Average value: 1.37 g/cc Grade Count:53 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Density | 1.23 - 1.62 g/cc | 0.0444 - 0.0585 lb/in³ | Average value: 1.39 g/cc Grade Count:45 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Lanxess Durethan® BKV 115 H2.0 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RL003 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL003 is a compound based on Nylon 66 resin containing PTFE. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
Taiwan Sheen Soon Sheenthane® D6010E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRILOY D20009 PC (Asia Pacific) LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A9720 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PA6/6 03002 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN® S3100 PC/ABS alloy Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D3165 |
Vicone High Performance Rubber VicoSil™ 0591EK-CL High Performance Silicone Rubber Information provided by Vicone |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM-D792 |
Polyram Polytron P40N01 Homopolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber A CHEMICALLY COUPLED 40% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 74/P Flexible PVC, Injection Molding for Footwear Pearl sandals |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 90 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM 15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Eurostar Staramide PF003U PA6, 15% Glass Fiber Filled, Injection Molded Staramide PF003U is an 15% Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin, UV Stabilized (also known as Staramide 6 15V S4)Information provided by Eurostar. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene CP0437T40V Copolymer Talc Reinforced Approved to GMP.PP.079 Black A12566 |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Conditioned) Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Density | 1.23 g/cc @Temperature 23.0 °C |
0.0444 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH T20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
DuPont Performance Polymers Neoprene AC MEDIUM Polychloroprene Rubber
(discontinued **) Description: Chloroprene polymer designed for use in high strength solution adhesives requiring rapid rates of strength development.Processing and Performance Features: Primary use is in contact adh.. |