Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram Polytron P40N01 Homopolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P40N01 Homopolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A CHEMICALLY COUPLED 40% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM-D792
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 125 MPa
18100 psi
ASTM-D638
Elongation at Break 2.65 %
2.65 %
ASTM-D638
Tensile Modulus 9.50 GPa
1380 ksi
ASTM-D790
Flexural Strength 175 MPa
25400 psi
ASTM-D790
Flexural Modulus 6.70 GPa
972 ksi
ASTM-D790
Izod Impact, Notched 2.00 J/cm

@Temperature 23.0 °C
3.75 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 152 °C
306 °F
ASTM-D648