Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.09 g/cc | 0.0394 lb/in³ | NCMT Method |
NCMT NanoPAC™ S202 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Density | 1.09 - 1.46 g/cc | 0.0394 - 0.0527 lb/in³ | Average value: 1.23 g/cc Grade Count:23 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Pyrotek J-9 Square Ceramic Rope AdvantagesExcellent Abrasion Resistance Fair Compression and Recall Information provided by Pyrotek. |
|||
Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0416 lb/in³ | |
Lord Adhesives 403 Flexible, High Impact and Peel Resistance, Fast Cure Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/A |
Solvay TECHNYL® B 230 PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/A |
Solvay TECHNYL® B 238 Black 21 N PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/A |
Solvay TECHNYL® C 536XT PA6, Conditioned Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermotuf R1000IX4 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Stellarchem MP-855WR TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Struktol POLYDIS 3610 Reactive, elastomer modified epoxy prepolymer (block-copolymer) Applications: STRUKTOL POLYDIS 3610 is used where conventional epoxy systems and prepolymers are unable to satisfy the demands of for example impact, flexural or peel strength.Information provided b.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/B |
Styron PULSEâ„¢ GX50 PC/ABS Engineering Resin Overview: PULSE GX50 engineering resins give exceptional impact strength even at low temperature and have sufficient heat resistance for the majority of automotive interior components. This resin pr.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Solvay SOPROPHOR® 796/85 Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOPROPOXYLATED POLYARYLPHENOL IN GLYCOL SOLUTIONCAS: 70880 – 56 – 7 ; 57 – 55 – 6Solubility: Solub.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | DIN 53479 |
Polyram PlusTek RA843 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | DIN 53479 |
Polyram PlusTek RA846 Nylon 6.6, Impact Modified Impact modified and heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183-87 |
Wellman Wellamid® XT1482-BK High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Loctite® Quick Set™ 404 Industrial Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Denka MALECCA K-700 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Eurostar Staramide R1000IX4 PA66, Impact Modified, Injection Molded Staramide R1000IX4 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI020 Star X 1020)Information provided by Eurostar. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NB50 NL IT PA 6 super tough Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
Adell BI-10 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Density | >= 1.09 g/cc | >= 0.0394 lb/in³ | |
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | AboCast 7802-1 |
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | AboCast 7802-1 |
Abatron AboCast 7802-1/AboCure 7804-4 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | AboCast 7802-1 |
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO data |
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Solvay RHODISOLV® RPDE Solvent Rhodiasolv RPDE is an environment friendly, biodegradable, non toxic, non ecotoxic, low VOC solvent.Identification: DIMETHYL GLUTARATE, DIMETHYL SUCCINATE, DIMETHYL ADIPATECAS: 627 – 93 – 0 / 1119.. |