Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE G 7821 Multi-Flex® high heat compounds are a new generations elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Kraton G technology and featur.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Plastcom SLOVALEN PC 63 T 15 PP reinforced with 15% mineral filler Features: Modified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Application in all automotive interior industry.D.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound PRE-ELEC® PP 1398 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Faradex MS003XXC PP (Europe-Africa-Middle East) LNP* Faradex* MS003XXC is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.This data was supplied by SABIC-IP for.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK15 is an SBC consisting of our developmental BK10 grade with a mold release added for easier processing. BK15 molded parts give excellent detail on f.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Solvay GERONOL® FF/4-E Surfactant Description: Multipurpose emulsifier for agrochemical formulations. Used in pair with Geronol FF/6-C or MS-C.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most pola.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized. |
|||
Density | 1.01 g/cc @Temperature 20.0 °C |
0.0365 lb/in³ @Temperature 68.0 °F |
Relative density |
Suqian Unitechem Light Stabilizer 944 Chemical Name: Poly-{[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidyl)imino]-1,6-hexanediyl[(2,2,6,6-tetramethyl-4-piperidyl)imino]}CAS NO.: 70624-18-9M.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Polyram PlusTek PD1002NT Nylon 12 for Extrusion Medium viscosity Nylon 12 for extrusion application.Information provided by Polyram. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: XK41 is an extrusion grade of K-Resin SB copolymer designed specifically for improved performance in blends with general purpose polystyrene. It is eas.. |
|||
Density | 1.01 g/cc @Temperature 240 °C |
0.0365 lb/in³ @Temperature 464 °F |
Melt |
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® L 20 L PA12 Product Description: Grilamid L 20 L is a medium viscosity Polyamide 12 (PA12) extrusion type. It is UV and heat stabilized. Its main features are: High surface quality Very good UV and heat resista.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® L 25 nat 6112 PA12 Product Description: Grilamid L 25 natural 6112 is a high viscous, Polyamide 12 extrusion grade. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378, Type PA 12-H. Application examples:.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Cytec EN-8 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Diamond Polymers NPP25-0802 GF20 20% Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. mold-release agent... |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO R 1183 D |
Arkema Group Rilsan® Clear G380 Renew Polyamide Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Zytel® LC6210 BK010 is a highly toughened, heat stabilized polyamide 612 for extrusion, blow molding or processing by other techniques requiring high melt viscosity. It was previously coded Zytel®.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Polyplastic Armlen® PP 12IM-895 Impact Modified Polypropylene Impact modified polypropylene composite materialUV resistantInformation provided by PolyPlastic Group. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Solvay RHODASURF® ID/79 Surfactant Identification: ETHOXYLATED ALCOHOLSolubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Biological activ.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Solvay RHODOLINE® HP Surfactant Description: Highly effective white oil defoamer for latex processing.Available in: Asia Pacific, Europe, Latin America and North America.Solubility: Dispersible in water. Soluble in most polar and .. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Arkema Group Pebax® MX 1205 Polyether Block Amide (PEBA) Typical application: Impact modifierInformation provided by Arkema Group |
|||
Density | 1.01 g/cc @Temperature 25.0 °C |
0.0365 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 1203 Specialty Polyol Description: Pluracol® 1203 is a conventional polyol with 2- and 3-functional characteristics. Pluracol1203 is specially designed for 1-component adhesives, foam-sealants, and microcellular elasto.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 2781 |
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |