Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE G 7821.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Multi-Flex® high heat compounds are a new generations elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Kraton G technology and feature excellent heat and ozone resistance. These products cover a wide temperature span from -50°C to 150°C. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Melt Flow 3.0 g/10 min
3.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
10 sec; ASTM D-2240
Tensile Strength, Ultimate 9.00 MPa
1310 psi
ASTM D638
Elongation at Break 660 %
660 %
ASTM D638
Flexural Modulus 0.0517 GPa
7.50 ksi
Secant 1%; ASTM D-790
Compression Set 20 %
20 %
for 22 hours at 23°C; ASTM 395
30 %

@Temperature 70.0 °C
30 %

@Temperature 158 °F
22 hours at 70°C; ASTM 395
48 %

@Temperature 100 °C
48 %

@Temperature 212 °F
22 hours at 100°C; ASTM 395