Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 2.20 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
ASTM D792
Polikim EFALON® T-100 Virgin PTFE
Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu..
Density 2.16 - 2.20 g/cc
0.0780 - 0.0795 lb/in³
ASTM D792-50
Mikro-Technik Reproflon PTFE
Reproflon is reclaimed PTFE scraps. The powder can be reused for the usual manufacturing procedures.Information provided by Mikro-Technik GmbH
Density 2.16 - 2.20 g/cc
0.0780 - 0.0795 lb/in³
Mikro-Technik Reproflon G25 PTFE
Available Forms: Rods, Tubes. Special Characteristics:Higher resistance to abrasionHigher resistance to compression compared to virgin PTFE and unfilled ReproflonReduced plastic flowInformation prov..
Density 1.20 - 2.20 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.0434 - 0.0795 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Palusol® 100 Silicate Panel
Relevant identified uses: Intumescent plates for use as fire protection in the building industryInformation provided by BASF
Density 1.20 - 2.20 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.0434 - 0.0795 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Palusol® 104 Silicate Panel
Relevant identified uses: Intumescent plates for use as fire protection in the building industryInformation provided by BASF
Density 1.90 - 2.20 g/cc
0.0686 - 0.0795 lb/in³
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 1.90 - 2.20 g/cc
0.0686 - 0.0795 lb/in³
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 1.20 - 2.20 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.0434 - 0.0795 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Palusol® 210 Silicate Panel
Relevant identified uses: Intumescent plates for use as fire protection in the building industryInformation provided by BASF
Density 2.00 - 2.20 g/cc
0.0723 - 0.0795 lb/in³
Molded
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound
BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Density 2.13 - 2.20 g/cc
0.0770 - 0.0795 lb/in³
ASTM D792
Guarniflon PTFE G200 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
apparent
Beijing Evergrow Resources PTFE Extrusion Tube
Features:PTFE extruded tubing is manufactured by high pressure PTFE dispense resin mixed with additive, it is extruded and sintered. According to different demands, the tubing could be opaque or tra..
Density 1.00 - 2.20 g/cc
0.0361 - 0.0795 lb/in³
Average value: 1.76 g/cc Grade Count:71
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
Density 2.13 - 2.20 g/cc
0.0770 - 0.0795 lb/in³
ASTM D792
Guarniflon PTFE G300 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..