Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | at RT |
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
Special Metals INCOLOY® Alloy 330 A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 2 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness Tensile strength (ultimate and yield), shear strength, and elongation values reported here are typical for Cold Rolled Sheet, 2 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness samples. Density a.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness Tensile strength (ultimate and yield), shear strength, and elongation values reported here are typical for Cold Rolled Sheet, 3 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness samples. Density a.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness Tensile and bearing strengths (ultimate and yield) and elongation values reported here are typical for Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness samples. Density and m.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Forged Disc, 2 Part Heat Treatment Tensile strength (ultimate and yield), reduction of area, and elongation values reported here are typical for Forged Disc, 2 Part Heat Treatment samples. Density and magnetic permeability are typica.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Forged Disc, 3 Part Heat Treatment Tensile strength (ultimate and yield), reduction of area, and elongation values reported here are typical for Forged Disc, 3 Part Heat Treatment samples. Density and magnetic permeability are typica.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Flat, 2 Part Heat Treatment, 1.250 inch (31.8 mm) Thickness Tensile strength (ultimate and yield), shear strength, compressive strength, reduction of area, and elongation values reported here are typical for Hot Finished Flat, 2 Part Heat Treatment, 1.250 in.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Rod, 3 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter Tensile strength (ultimate and yield), shear strength, reduction of area, and elongation values reported here are typical for Hot Finished Rod, 3 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter s.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
Special Metals UDIMET® alloy 720 Nickel Base Alloy UDIMET® alloy 720 is a nickel base alloy, solid solution strengthened with tungsten and molybdenum and precipitation-hardened with titanium and aluminum. The alloy combines high strength with me.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
Carpenter 20Cb-3® Stainless Steel, Strip, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
ATI Allegheny Ludlum AL 20™ Plate Specialty Steel The N08020 alloy has been available for many years and has found applications in many environments, such as in chlorides and in sulfuric and sulfurous acids.Although AL 20 alloy was developed for im.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
ATI Allvac® 706 Nickel Superalloy, Heat Treatment: 954°C (1750°F) + Age Data provided by Allvac.Applications: Land based turbine wheels and spacers. Jet engine components. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
ATI Allvac® 720 Nickel Superalloy, Heat Treatment: 1093°C (2000°F) + Age Data provided by Allvac.Applications: Wheels, jet engine turbine discs and blades. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
ATI Allegheny Ludlum AL 800AT™ Nickel-Base Alloy, UNS N08811 AL 800AT alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-co.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
ATI Allegheny Ludlum AL 800H™ Nickel-Base Alloy, UNS N08810 AL 800H alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-cor.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 2 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness Tensile and bearing strengths (ultimate and yield) and elongation values reported here are typical for Cold Rolled Sheet, 2 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness samples. Density and m.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | Precipitation Hardened |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Rod, 2 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter Tensile strength (ultimate and yield), shear strength, reduction of area, and elongation values reported here are typical for Hot Finished Rod, 2 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter s.. |
|||
Density | 8.08 g/cc | 0.292 lb/in³ | |
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |