Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.77 g/cc | 0.0640 lb/in³ | |
Parkway Products Thixomolded® AM50A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides.. |
|||
Density | 1.77 g/cc | 0.0640 lb/in³ | Yield Density |
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film
(discontinued **) Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 2950 PVDF Copolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
SGL Carbon Group EK 2209 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Conditioned) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 0177 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Techmer ES HiFill® PVDF CF15-M BK 15% Milled Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in .. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Plenco 6500 Phenolic, Briquette, Injection Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65 Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
Cytec Thornel® T-650/35 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ISO 1183 |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.77 g/cc | 0.0640 lb/in³ | ASTM D792 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
Arkema Group Kynar® 1000 HDC N 118 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1C,P.?E5.I.B.E.C,, ?(1.5-2.5)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, hig.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
Arkema Group Kynar® FLEX 2821 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (2.5-6.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousn.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
Arkema Group Kynar® FLEX 2822 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (4-8)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness .. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | Nominal Laminate |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581 Fiber: E-Glass, Weave: 8HS, 300 g/m2Information provided by HexCel |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D-792 |