Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 7518 C Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Plenco 50130 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Plenco 51130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L 9512 PPS, 45% Glass Fiber
(discontinued **) Good-flow Embedding Compound. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Embedding of Microchips and Electronic ComponentsProcessing: Injection Molding (Melt Temp.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 50009 Anti-split CPP. 70% CaCO3 Filled.Carpet Backing.Information provided by Multibase |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. |
|||
Density | 1.72 g/cc @Temperature 25.0 °C |
0.0621 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® SV135 PFPE Solvent Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hGR50 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific) LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific) LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Plenco 6015 Phenolic, Briquette, Transfer Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
DSM Arnite® TV4 290 PBT-GF50 50% Glass Reinforced |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-61L Compression Molded PPS Compound, 25% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | |
BASF Paliotol™ Yellow L 2140 Color Additive Description: Isoindoline yellow with high opacity and reddish shade for OEM and industrial coatings.Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, A.. |
|||
Density | 1.72 - 1.94 g/cc | 0.0620 - 0.0700 lb/in³ | ASTM D792 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Density | 1.72 - 1.94 g/cc | 0.0620 - 0.0700 lb/in³ | ASTM D792 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Conditioned, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Density | 1.72 - 1.94 g/cc | 0.0620 - 0.0700 lb/in³ | ASTM D792 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Density | 1.72 - 1.94 g/cc | 0.0620 - 0.0700 lb/in³ | ASTM D792 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66 LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |