Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.64 - 1.65 g/cc | 0.0592 - 0.0596 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 65-1 Linear Low Density Polyethylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RX01075 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX01075 is a compound based on Nylon 66 resin containing PTFE, Mineral. Added features of this material include: Heat Stabilized. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA12 LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing 50% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East) VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® SHF4960 PBT Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH |
3M AC-236 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class A are brushable, two-component, liquid polysulfide polymer sealant providing excellent fuel tank and fuselage seals. They have outstanding resistance to aviation ga.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH; AMS3276 |
3M AC-275 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH; AMS3276 |
3M AC-275 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
A. Schulman ComAlloy Hiloy® 433 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.64 g/cc @Temperature 23.0 °C |
0.0592 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-MFC-G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
BASF Heligoen® Blue L 6975 F Color Additive Description: Brilliant a-phthalocyanine blue with high color strength and excellent rheology in systems containing aromatic solventsChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: Po.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE5264 NC010 PET
(Unverified Data**) Rynite® RE5264 NC010 is a 36% glass fiber reinforced, color stabilized, modified polyethylene terephthalate.Information provided by DuPont Performance Polymers |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America FS-4 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owen.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |