Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Lanxess Pocan® T 7331 POS151 000000 PBT + PET, 30% Glass Fiber
(discontinued **) PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Pasargad Polymer Peyvand Pasamid 3P-H2150B Nylon 66, 50% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Density | 1.55 - 1.59 g/cc | 0.0560 - 0.0574 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 325 Rigid PVC, Extrusion Lead Free Verticle curtains |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON WSF42 PBT (Europe-Africa-Middle East) LNP*STAT-KON* WSF42 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Stainless Steel Fiber. Added features include: Electrically Conductive. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PC GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM A792 |
PlastxWorld Veroplas PB3301F Nylon 66 flame retarded (UL94 V0), 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
DSM Arnite® TV4 461 (PBT+PET)-GF30 30% Glass Reinforced |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.55 - 1.59 g/cc | 0.0560 - 0.0574 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 88 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Addiplast Addinyl B2 V50 Nylon 6, 50% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® 551GT20S PBT Resin Glass fiber and mineral filled, flame retardant, low warpage, superior electrical performance, surface glossInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® PE126 PET Polyester, 30% Glass Reinforced PET Polyester, with 30% glass reinforcement.Data provided by the manufacturer |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
LATI Latiohm 75/4-08 PD01 G/30 PBT, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |