Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.47 g/cc | 0.0531 lb/in³ | STN 64 0111 |
Plastcom SLOVAMID 6 GF 40 Polyamide 6, 40% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 40% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Kadel® E-1130 Polyketone
(discontinued **) High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r.. |
|||
Density | 1.47 - 1.61 g/cc | 0.0531 - 0.0582 lb/in³ | Average value: 1.52 g/cc Grade Count:12 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 115 Rigid PVC, Extrusion Lead Free Small tubes for shoes |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 317/UV Rigid PVC, Extrusion Lead Free Profiles anti-UV |
|||
Density | 1.47 g/cc | 0.0532 lb/in³ | |
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Density | 1.47 g/cc | 0.0530 lb/in³ | |
Industrial Laminates/Norplex MC330 Cotton Fabric Description: Grade MC330 is a cotton cloth/phenolic resin composite which is specially processed to be used in cryogenic applications. Such applications include spacers for installation of liquid ox.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GB40 HS BK 40% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackInforma.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific) LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66 LNP THERMOCOMP* RF008XXZ is a compound based on Nylon 66 resin containing 40% Glass Fiber. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RFB53SUZ PA 66 LNP THERMOCOMP* RFB53SUZ is a compound based on Nylon 66 resin containing Glass Bead, Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, Conditioned Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TC551 PA46 FR(17) Thermal conductive material, Flame Retardant |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50 Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
Eurotec® Tecoform® PO20 GR10 NL HS POM, 10% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 3621 Halogen Free PVC General purpose |
|||
Density | 1.47 - 1.51 g/cc | 0.0531 - 0.0546 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 211 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation and sheathing, improved processabilityInformation provided by Fainplast Compo.. |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural Information provided by Eurotec® |
|||
Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg.. |